access icon free Ductile dicing of LiNbO3 ridge waveguide facets to achieve 0.29 nm surface roughness in single process step

A single-step ductile dicing process capable of manufacturing optical quality facets in lithium niobate (LiNbO3) ridge waveguides with an average surface roughness of 0.29 nm is reported. This result is comparable with surface roughnesses achieved by lapping and polishing and represents an order of magnitude improvement over the prior state of the art in LiNbO3 waveguide facet dicing.

Inspec keywords: lithium compounds; ridge waveguides; surface roughness

Other keywords: ridge waveguide facets; optical quality facet manufacture; LiNbO3; lithium niobate ridge waveguides; single process step; surface roughness; single-step ductile dicing process

Subjects: Waveguides and microwave transmission lines

References

    1. 1)
    2. 2)
    3. 3)
    4. 4)
    5. 5)
    6. 6)
    7. 7)
    8. 8)
http://iet.metastore.ingenta.com/content/journals/10.1049/el.2017.2863
Loading

Related content

content/journals/10.1049/el.2017.2863
pub_keyword,iet_inspecKeyword,pub_concept
6
6
Loading
Correspondence
This article has following corresponding article(s):
in brief